Home > News

Why Does Platinum-Cured Silicone Not Require Post-Curing?

2026-10-10

Why Does Platinum-Cured Silicone Not Require Post-Curing?

Breaking Down the Principle Behind Platinum Vulcanization

With the implementation of the new Chinese national standard GB 4806.16-2025, more and more manufacturers are choosing platinum-cured, post-curing-free silicone rubber for food-contact applications.

Many mold technicians, purchasing managers, and engineers have the same question:

For conventional peroxide-cured silicone rubber, products usually need to be post-cured at around 200°C for several hours after compression molding.

So why can platinum-cured silicone rubber be molded and used after a single curing process, without secondary baking?

Some people simply assume that it is because “special additives” have been added to the formulation. Others wonder:

If there is no post-curing, where do the low-molecular-weight substances and curing by-products go?

Today, let's put aside complicated academic formulas and explain platinum-cured silicone from three fundamental perspectives:

crosslinking mechanism, differences in by-products, and VOC control.

This will help explain why post-curing-free platinum silicone is naturally well suited to the new food-contact requirements.


01

How Does Platinum-Cured Silicone Work?

Addition-Cure Reaction with Virtually No By-Products

Post-curing-free silicone is formally known as platinum-catalyzed addition-cure silicone rubber.

The core components of the system are:

1. Vinyl silicone rubber:
‎A silicone rubber polymer containing vinyl groups along its molecular chains.

2. Hydrogen-containing silicone oil:
‎The crosslinking agent, which provides Si-H bonds.

3. Platinum catalyst:
‎A platinum complex that catalyzes the curing reaction.

How does the reaction work?

Under heat, the platinum catalyst promotes a hydrosilylation reaction.

The Si-H bonds in the hydrogen-containing silicone oil react directly with the vinyl groups on the silicone polymer chains. This connects different polymer chains and forms a stable three-dimensional crosslinked network.

✅ The key difference

An addition-cure reaction directly forms chemical bonds between the components. It does not rely on decomposition of a curing agent and therefore produces virtually no volatile decomposition by-products.

After the reaction, the platinum catalyst mainly functions as a catalyst. It accelerates the reaction without being consumed as a reactant and does not itself generate volatile gases.

The key takeaway:

Conventional peroxide-cured silicone:
‎Curing involves decomposition of the peroxide curing agent → volatile by-products are generated → post-curing is commonly required to remove residual volatiles.

Platinum-cured silicone:
‎Curing occurs through an addition reaction → virtually no curing by-products are generated → post-curing may not be necessary when the formulation and process are properly controlled.


02

Why Does Post-Curing-Free Platinum Silicone Have Low VOM?

And Why Is It Suitable for GB 4806.16?

The new standard introduces requirements related to VOM (Volatile Organic Matter).

In practical terms, VOM testing evaluates volatile substances that can be released from silicone materials under specified high-temperature testing conditions, including residual low-molecular-weight siloxanes and other volatile substances.

The low VOM level of a platinum-cured system comes from two levels of control:

1. No curing by-products are generated during crosslinking

The crosslinking reaction itself does not generate the same type of volatile decomposition products associated with peroxide curing.

This removes a major potential source of volatile substances at the source.

2. Low-molecular-weight substances are controlled through raw-material selection

High-quality platinum-cured silicone formulations typically use carefully selected silicone polymers, fillers, and other raw materials with controlled levels of residual low-molecular-weight siloxanes.

This means the overall volatile content can be kept significantly lower than that of conventional systems when the formulation and manufacturing process are properly designed.

Therefore, after a single molding and curing process, there may be very little residual volatile material that needs to be removed by additional baking.

For properly formulated and processed materials, VOM levels can potentially be controlled to approximately 0.1–0.2%, well below a 0.5% limit where applicable, while also supporting compliance with requirements such as LFGB and FDA, subject to the specific formulation, test method, and finished-product testing.

⚠️ Common misconception:

“Post-curing-free” does NOT mean “zero low-molecular-weight substances.”

This point is important.

All silicone rubber materials can contain trace amounts of cyclic siloxanes and other low-molecular-weight substances, which may originate from the silicone polymer itself and from the raw-material manufacturing process.

Therefore, post-curing-free platinum silicone does not mean that the material contains absolutely no volatile substances.

Rather, it means that:

the curing reaction itself does not generate the same type of additional volatile decomposition by-products, while careful raw-material selection and process control can further reduce the overall volatile content.

In other words:

Low VOM ≠ zero VOM.


03

What Should You Watch Out for When Using Platinum-Cured Silicone?

Understanding the curing mechanism is only half the story.

In actual production, platinum-cured silicone has several important processing requirements, and many manufacturing problems come from these areas.

1. Platinum catalyst inhibition

Platinum catalysts are highly sensitive to certain contaminants.

Substances containing sulfur, nitrogen, phosphorus, tin, and certain heavy metals can inhibit or “poison” the platinum catalyst.

This may result in:

incomplete curing

poor surface curing

sticky surfaces

reduced mechanical properties

unstable production performance

Therefore, the mixing equipment, molds, release agents, gloves, and production environment must be kept clean and free from potential contaminants.

Cross-contamination should also be avoided.

In particular, equipment used for peroxide-cured silicone should generally not be directly shared with platinum-cured silicone without proper cleaning and process control.

2. Curing temperature window

Platinum-cured silicone can begin curing at relatively low temperatures.

Typical molding temperatures may be around 110–140°C, depending on the formulation, product thickness, mold design, and curing system.

If the temperature is too high, premature crosslinking or scorch can occur.

If the temperature is too low, curing may be incomplete.

Therefore, the curing temperature, mold temperature, pressure, and molding time must be properly matched to the specific silicone formulation.

3. Higher raw-material cost

Platinum catalysts are expensive, so platinum-cured silicone generally has a higher material cost than conventional peroxide-cured silicone.

However, material price alone should not determine the choice.

The total production cost should also include:

oven electricity

labor

post-curing time

post-curing defects

rework

testing costs

production lead time

For thick-walled products, large silicone components, and export orders with strict food-contact requirements, platinum-cured silicone can provide a better overall cost-performance balance.


04

Peroxide-Cured vs. Platinum-Cured Silicone

A Quick Comparison

Item

Conventional Peroxide-Cured Silicone

Platinum-Cured Silicone

Curing mechanism

Free-radical curing

Hydrosilylation / addition curing

Main curing agent

Organic peroxide

Hydrogen-containing silicone + platinum catalyst

Curing reaction

Decomposition and crosslinking

Direct addition and crosslinking

Curing by-products

Volatile decomposition by-products may be generated

Virtually no curing by-products

Post-curing

Commonly required

Often unnecessary when properly formulated and processed

Typical molding temperature

Higher

Approximately 110–140°C, formulation dependent

Catalyst sensitivity

Relatively lower

Highly sensitive to sulfur, phosphorus, nitrogen, tin, etc.

Material cost

Lower

Higher

VOM control

Requires additional post-curing and raw-material control

Naturally advantageous, but raw-material and process control are still required

Food-contact applications

Suitable with proper formulation and testing

Particularly suitable for low-VOM applications


05

Conclusion

Conventional peroxide-cured silicone generates volatile decomposition by-products during curing, which is why post-curing is commonly used to drive out residual volatiles.

By contrast, platinum-cured silicone uses an addition-crosslinking mechanism. The curing reaction itself generates virtually no volatile decomposition by-products.

That is the fundamental reason why, with a properly designed formulation and controlled manufacturing process, post-curing may not be necessary.

As food-contact regulations become increasingly stringent, low VOM is becoming an increasingly important requirement for food-grade silicone products.

When selecting silicone materials, manufacturers should therefore look beyond the material price alone.

Understanding the underlying curing chemistry can help manufacturers:

select the right silicone system;

optimize molding processes;

reduce VOC/VOM-related risks;

improve production efficiency;

and reduce the risk of unexpected testing failures.

In the era of stricter food-contact standards, choosing the right curing system is not simply a matter of cost — it is a matter of material chemistry, production control, and product compliance.